Cura Profile / Settings to Download for Kingroon KP3S

In this article, we'll guide you through to work out the best Cura profile for our Kingroon KP3S 3D printer. The profile would cover key values in Cura settings for the print of the most common 3D print material PLA, ABS, and TPU filaments. 

How to Set Cura Profile on the Software

You can access to the Cura profile through the following steps:

Preferences > Printers > Add Printer > Add a non-networked printer.

Scroll to “Kingroon”, expand the section, and select Kingroon KP3S or Kingroon KP3.

Cura profile kingroon kp3s

Now you already accessed to the basic Cura settings for your printer. 

PLA Cura Profile for Kingroon KP3S

Cura profile for PLA filament to DOWNLOAD.

Printing temperature: 200 °C
Bed temperature: 60 °C
Speed: 50 mm/s
Layer height: 0.12 mm
Retraction: 1 mm at 40 mm/s
Infill: 20%
Initial layer speed: 20 mm/s
Initial fan speed: 0%

Kingroon KP3S PLA Cura Profile

ABS Cura Profile for Kingroon KP3S

Basics about ABS filament

ABS is an abbreviation for acrylonitrile butadiene styrene, a material with great mechanical properties and higher temperature resistance. ABS filament is more often used in prototyping and printing functional parts. 

Tips for 3D print with ABS

Before printing with ABS filament, you should be aware of these things.
1. ABS filament is hydroscopic; always keep your ABS filament dry in a dry box
2. ABS filament is sensitive to changing ambient temperature; place your 3D printer inside an enclosure, and your 3D print with ABS will be more stable.
3. ABS filament doesn't stick well to print bed and tends to warp; always use a glue stick and apply some glue (or ABS slurry) onto the print bed when print with ABS.

Important parameters for ABS printing on KP3S

Printing Temperature:240℃
Initial Printing Temperature:250℃
Build Plate Temperature:100℃
Build Plate Temperature Initial Layer:100℃
Retraction Distance: 1.0mm
Retraction Speed: 20mm/s
Cooling: Off
Build Plate Adhesion: Brim

1. Set higher printing and bed temperatures

Comparing with PLA, ABS filament needs much higher printing temperature to melt and higher build temperature. It's tested that 240℃ for printing temperature, 250℃ for initial printing temperature, 100℃ for build plate temperature are suitable for ABS printing on KP3S. You can try these temps on other printers and adjust according to the result.

2. Set lower retraction speed

For retraction settings, the retraction distances for PLA and ABS printing are the same. But much lower retraction speed is needed for ABS printing. 20mm/s is recommended to print ABS on KP3S, while the retraction speed for PLA printing reaches 80mm/s.

3. Turn off fan cooling

Blower fan near the nozzle produces temperature gradients and leads to temperature differences. These greatly affect printing qualities with ABS filament. Make sure cooling is disabled to proceed.

ABS Profile

4. Use "Brim" to ensure build plate adhesion

ABS filament does not stick to build plate well. To assist with build plate adhesion while printing ABS, never forget to select "Brim" as "Build Plate Adhesion Type".

ABS Profile

TPU Cura Profile for Kingroon KP3S

Basics about TPU filament

TPU is an abbreviation for thermoplastic polyurethane, a flexible and abrasion resistant thermoplastic. TPU filament offers many benefits for 3D printed parts, which are flexible, durable, resistant to chemicals and withstand up to 80℃ ambient temperature.

Tips for 3D print with TPU

Printing with TPU also requires more than with PLA. Before you proceed, be aware of below things.

1. 3D printer with direct drive extruder is more preferred for TPU printing than a Bowden 3D printer, which makes Kingroon KP3S a good option. A Bowden extruder connects to the hotend with a long PTFE tube, which means a long distance for the filament to travel into the hotend; on the other side, a direct drive extruder is mounted directly onto the hotend, simply pushing the filament to the nozzle. Shorter distance means less filament clog, coil, and some issues that would happen on soft and flexible filament like TPU. 

2. Similar to ABS filament, TPU filament absorbs moisture quick and it's better to be kept in a dry box.

Important Cura Settings for TPU printing on KP3S

Cura Profile for TPU filament to DOWNLOAD.

Layer Height: 0.2mm
Initial Layer Height: 0.28mm
Infill Density: 8%
Printing Temperature:220℃
Initial Printing Temperature:220℃
Build Plate Temperature:40℃
Build Plate Temperature Initial Layer:40℃
Print Speed: 35mm/s
Retraction Distance: 3.5mm
Retraction Speed: 40mm/s

1. Use appropriate layer height

As we tested, using 0.2mm layer height and 0.28mm initial layer height offers better result when printing TPU with KP3S. You can slightly vary these values and test out the best result for your printer.

2. Set lower infill density

Lower infill density is crucial to retain your 3D print with great flexibility as your raw TPU filament. For this purpose, infill density around 8% is recommended here.

3. Medium printing temperature but lower build temperature

The printing temperatures for TPU filament is just in the middle of PLA and ABS printing. On the Kingroon KP3S, 220℃ is just the right value.

But for the build plate, lower temperatures are much friendlier for TPU filament. It is understandable when takes the softness of TPU into consideration.

4. Apply longer retraction distance

Unlike ABS printing, a longer retraction distance of 3.5mm is recommended for TPU printing on KP3S.

5. No Raft for TPU printing

When printing with TPU, never select "Raft" as the build plate adhesion type. Enabled Raft means higher extrusion rate on the bottom layer, which leads to various problems.  

PETG Cura Profile for Kingroon KP3S

Basics about PETG filament

PETG is a great material to replace ABS. It is highly recommended if you are longing for some material to print parts or accessories that require durability and high strength. Compare with ABS, PETG is much easier to print. It requires no enclosure and prints with no bad smell.  

Tips for 3D print with PETG

PETG is quite sticky, so stringing would be a huge problem. So you might want to close the “Z hop” and turn on “Avoid Printed Parts When Traveling” and “Avoid Supports When Traveling”. 

On the other hand, using some glue or the LAC Spray is another trick to print well. 

Important parameters for PETG printing on KP3S

Printing Temperature:235℃


Initial Printing Temperature:235℃


Build Plate Temperature:75℃


Build Plate Temperature Initial Layer:75℃


Retraction Distance: 1.0mm


Retraction Speed: 40mm/s


Cooling: On

Fan Speed:20%-40%

Cura Profile for PETG filament to DOWNLOAD.

 

Test Print Files to Download for Kingroon KP3S

Artículo anterior Kingroon KP3 Firmware Download
Artículo siguiente Add Laser Head on Kingroon KP3S 3D Printer

Comentarios

Kingroon 3D Official - junio 24, 2022

@Ismenc

Thanks for your comment and let us know your problem.

Of course when you changed to a 0.8mm nozzle, you should adjust parameters when slicing the STL file for your print. IF it still won’t fix the problem, then you need to tune the PID settings.

But as we tested, with a 0.8mm nozzle, stringing tends to happen. And there is no need to use a nozzle larger than 0.6mm.

Also we’ll provide tutorial over PID tuning for 0.8mm nozzle in the coming days. If it’s available, we’ll notice you ASAP.

Kind regards,
Kingroon Tech

Kingroon 3D Official - junio 24, 2022

@omar
Thanks for your comment and let us know your problem.

Please email us pictures or videos over the print failure issue on your KP3S, and also screenshots of your order information to our tech team via support@kingroon.com.

Our tech team will contact you ASAP and provide you the best solution for this issue.

Wish you a good day!

Alecio Araujo - mayo 26, 2022

Qual o CNPJ da empresa

Kingroon 3D Official - abril 4, 2022

@alex
We’re so sorry to hear that. Would you pls replace the old version of Cura to try?

alex - marzo 31, 2022

my kingroon kp3 is not recognized by Ultimaker Cure (latest version). The PC sees the serial port! Windows 10 pro. What to do ?

Kingroon 3D official - marzo 19, 2022

@omar
We’re so sorry for that, could you pls replace another SD card to try?

Kingroon 3D official - marzo 19, 2022

@Ismenc
If you change the nozzle, just need to change the thickness

omar - marzo 14, 2022

Hi
I have an KP3S board STM32F103 V1.2
Each time i generate the gcode file (Cura V14.13.1) and when start the printing from sd card
the printer restart and don’t print!? try again same problem
I tried different files same problem
What shall i do?

Ismenc - marzo 2, 2022

Hi.
How should parameters be adjusted when you change nozzle?
I got nice results when i switched to 0.6mm but when i tested 0.8mm i got insane stringing. Should PID’s be adjusted?